FIELD: well drilling. SUBSTANCE: injected in well in two portions is bridging material. First portion contains cement, calcium chloride and water, and the second portion contains synthetic latex and ucramine - surfactant based on neutralization product of fatty and naphthenic acids with amino compounds. Additionally injected between portions of bridging material and after injection of bridging material is fresh water. Bridging material is injected until building up the pressure of 5 MPa. Initial ingredients of bridging material are used in the following amounts, mas. cement 67, 84; calcium chloride 3.0; synthetic latex 2.0; ucramine 0.02; water 27, 14. EFFECT: higher efficiency. 2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FORMATION ISOLATION WITH CEMENT-SILICATE MUD | 2012 |
|
RU2519262C1 |
METHOD OF STABILIZING WELLS UNDER CONDITIONS OF HIGH-PRESSURE WATER MANIFESTATIONS | 0 |
|
SU1613581A1 |
METHOD FOR REPAIR INSULATION WORK USING SUSPENSIONS OF FINE MINERAL BINDER | 2015 |
|
RU2582143C1 |
METHOD OF CEMENTING CASING STRING IN WELL | 2023 |
|
RU2823955C1 |
WATER SHUT OFF METHOD | 2008 |
|
RU2374428C1 |
METHOD OF SEALING RECOVERY OF PRODUCTION STRING | 2010 |
|
RU2455458C1 |
METHOD FOR REPAIR AND INSULATION WORKS IN WELL | 2018 |
|
RU2684932C1 |
METHOD FOR CEMENTING THE CONDUCTOR, A TECHNICAL COLUMN DURING THE CONSTRUCTION OF WELLS | 2022 |
|
RU2792128C1 |
METHOD TO RECOVER TIGHTNESS OF PRODUCTION COLUMN | 2011 |
|
RU2463436C1 |
METHOD OF INSULATING WATER-DEVELOPMENT STRATA | 1997 |
|
RU2152507C1 |
Authors
Dates
1995-11-27—Published
1992-05-28—Filed