FIELD: building industry. SUBSTANCE: polymer-concrete mixture has, wt. -% unsaturated polyester resin 8.4-15; cobalt naphthenate 0.4-0.8; initiating agent of peroxide type 0.2-0.5; modifying agent unsaturated carboxylic acid glycidyl esters 1.0-1.7, and filler the rest. Filler is natural stone or glass processing waste, or their mixture at particle size less 20 mm at the ratio 80: 20, or a mixture of natural stone processing waste and glass working abrasive waste at particle size 0.09 (not above) at the ratio 85:15, or a mixture of natural stone processing waste, glass and glass working abrasive waste at the ratio 80:5:15. Mixture mobility is up to 8 cm, compression strength is up to 1596 kgs/cm2. EFFECT: enhanced quality of mixture. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| POLYMER-CONCRETE MIXTURE | 1992 | 
 | RU2049751C1 | 
| POLYMER COMPOSITION | 2002 | 
 | RU2270217C2 | 
| POLYMER-CONCRETE COMPOSITION FOR FACING SLABS | 1997 | 
 | RU2126775C1 | 
| METHOD OF POLYMER-CONCRETE MIXTURE PRODUCING | 1996 | 
 | RU2100303C1 | 
| POLYMER-CONCRETE COMPOSITION | 0 | 
 | SU1428733A1 | 
| POLYMER-CONCRETE COMPOSITION | 0 | 
 | SU1428734A1 | 
| COMPOSITE MATERIAL FOR FRONT PANELS | 2006 | 
 | RU2307808C1 | 
| POLIMER CONCRETE MIXTURE | 0 | 
 | SU1328330A1 | 
| POLYMER-CONCRETE MIX | 0 | 
 | SU1571026A1 | 
| POLYMER-CONCRETE MIX | 0 | 
 | SU1474131A1 | 
Authors
Dates
1995-12-10—Published
1992-07-22—Filed