FIELD: electrovacuum instrumentation engineering. SUBSTANCE: for joining metal frame to fiber-optic plate by soldering through glass-crystal layer preformed as soldering ring followed by its sintering, glass-crystal material is sintered and vitrified at complete melting temperature of glass-forming components with exposure to this temperature for 1-2 min. EFFECT: improved mechanical and thermal strength of photoelectronic device. 6 dwg
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF MANUFACTURE OF FIBRE-OPTICAL UNIT OF PHOTOELECTRON DEVICE | 1991 |
|
SU1819040A1 |
PROCESS OF MANUFACTURE OF FIBRE-OPTICAL UNIT OF PHOTOELECTRIC DEVICE | 1985 |
|
SU1336834A1 |
ULTRA-HIGH VACUUM HEAT-RESISTANT VIEWING WINDOW | 2020 |
|
RU2742506C1 |
METHOD FOR ACCELERATED TESTS OF ELECTROOPTICAL TRANSDUCER | 1991 |
|
RU2024097C1 |
PROCESS OF MANUFACTURE OF PHOTOELECTRON DEVICE | 1991 |
|
SU1780445A1 |
METHOD OF MAKING OPTICAL-MECHANICAL MODULE | 2009 |
|
RU2394258C1 |
METHOD FOR SEALING VACUUM ENCLOSURE OF X-RAY OPTICAL CONVERTER | 1999 |
|
RU2149479C1 |
METHOD OF PRODUCTION OF OPTICAL PIECES WITH ASPHERIC SURFACES | 2003 |
|
RU2245852C1 |
METHOD OF PRODUCING FIBRE-TEXTURED GLASS CERAMICS | 2009 |
|
RU2422390C1 |
VACUUM JACKET OF X-RAY ELECTRON-OPTICAL CONVERTER | 1998 |
|
RU2152100C1 |
Authors
Dates
1996-05-27—Published
1992-08-21—Filed