FIELD: manufacture of articles of construction purpose. SUBSTANCE: composition comprises (wt parts): 67-73 thermostabilized polyhexamethylane adipamide at ratio of carboxy and amine groups of 1.2:1 to 1.8:1; 0.2-0.5 bisphenolic antioxidant; 0.2-0.5 sterically hindered hydrolysis resistant triaryl phosphite; 0.25-0.6 oligocarbodiimide; 27-33 glass fiber. EFFECT: improved properties of the composition. 4 cl
| Title | Year | Author | Number |
|---|---|---|---|
| THERMOPLASTIC POLYMER COMPOSITION | 1991 |
|
RU2010819C1 |
| POLYAMIDE COMPOSITION | 1993 |
|
RU2063406C1 |
| POLYMERIC COMPOSITE MATERIAL | 1998 |
|
RU2144050C1 |
| METHOD OF REACTOR CLEANSING FOR ESTER SYNTHESIS | 1992 |
|
RU2011444C1 |
| POLYMER COMPOSITION | 1992 |
|
RU2032948C1 |
| PROCESS FOR PREPARING PLASTICIZERS | 1992 |
|
RU2034826C1 |
| ANTIFRICTION COMPOSITION | 1992 |
|
RU2016002C1 |
| POLYMER COMPOSITION | 1992 |
|
RU2028337C1 |
| ELECTROCONDUCTIVE POLYMERIC COMPOSITION | 1992 |
|
RU2016424C1 |
| POLYMERIC COMPOSITION | 1992 |
|
RU2016010C1 |
Authors
Dates
1996-10-10—Published
1991-08-28—Filed