FIELD: manufacture of building structures. SUBSTANCE: quality of binder can be improved by improving early strength and grade also by using wider range of raw materials and industrial waste to manufacture binder. Claimed binder comprises (wt%): 74-81 granular blast furnace slag; 15-20 neutralized phosphorus gypsum; 4-6 fine lime mild production waste which result from lime mild production. Specific surface area of individually or jointly crushed slag, phosphorus gypsum and fine slaking remnants is 3000-3500 sq.cm/g. Compression strength of samples of cement paste of standard density and standard hardening of 7 days and 28 days are 15-23 and 34-43.8, respectively. EFFECT: enhanced strength. 4 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| BINDER COMPOSITION | 0 | 
									
  | 
                SU1470698A1 | 
| CRUDE MIXTURE FOR PRODUCING GYPSUM BINDER AND ARTICLES FROM SAID BINDER | 2009 | 
									
  | 
                RU2413688C2 | 
| DECORATIVE SLAG CEMENT | 2002 | 
									
  | 
                RU2232139C1 | 
| CRUDE MIXTURE FOR MAKING CONSTRUCTION ARTICLES BASED ON NON-FIRED TECHNOLOGY | 2015 | 
									
  | 
                RU2584018C1 | 
| ADAPTIVE SYSTEM FOR CONTROLLING THE PROCESS OF PREPARATION OF SLAKED LIME | 1991 | 
									
  | 
                RU2027765C1 | 
| METHOD OF GRANULATION OF BLAST FURNACE SLAG | 0 | 
									
  | 
                SU1759800A1 | 
| BINDING AGENT | 2010 | 
									
  | 
                RU2476392C2 | 
| BINDING AGENT | 2004 | 
									
  | 
                RU2255063C1 | 
| METHOD OF GYPSUM BINDER MAKING | 0 | 
									
  | 
                SU1794913A1 | 
| BINDING AGENT | 1993 | 
									
  | 
                RU2087439C1 | 
Authors
Dates
1997-03-27—Published
1993-07-23—Filed