FIELD: oil and gas production. SUBSTANCE: parts are preliminarily treated with beads 0.4-0.8 mm in diameter, subjected to nitrocementation at 500-600 C for 4-6 h and then to oxide formation effected by cooling parts after nitrocementation in water. EFFECT: increased resistance to fatigue destruction, corrosion, and wear. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STEEL PARTS MANUFACTURE | 2000 |
|
RU2194794C2 |
METHOD OF THERMOCHEMICAL TREATMENT OF STEEL ARTICLES | 2011 |
|
RU2478137C2 |
METHOD OF THERMOCHEMICAL TREATMENT OF PIPE INTERNAL SURFACE OF LOW-CARBON STEEL | 1994 |
|
RU2081205C1 |
METHOD AND COMPOSITION FOR CARBO-CHROMIZING OF STEEL ARTICLES | 2004 |
|
RU2285741C2 |
METHOD OF CHEMICAL HEAT TREATMENT OF WORKPIECE FROM ALLOYED STEEL | 2016 |
|
RU2627551C1 |
METHOD OF PRODUCING ARTICLES OF STEEL AND ALLOYS | 0 |
|
SU1504270A1 |
PROCESS DETERMINING CORROSION RESISTANCE OF DIFFUSION LAYER OF PART FROM STRUCTURAL STEEL | 1993 |
|
RU2090861C1 |
METHOD OF CHEMICAL HEAT TREATMENT OF PART FROM ALLOYED STEEL | 2014 |
|
RU2559606C1 |
METHOD AND AUTOMATIC LINE FOR CHEMICAL-THERMAL TREATMENT OF STEEL PARTS | 0 |
|
SU1775481A1 |
METHOD OF OXIDIZING IRON-CARBON ALLOYS | 1996 |
|
RU2110603C1 |