FIELD: metallurgy; chemical-thermal treatment of articles.
SUBSTANCE: proposed method includes successive case-hardening and chromizing in fluidized layer. For case-hardening of articles use is made of mixture containing the following components, mass-%: charcoal, 5-30; water, 5-10; the remainder being corundum. Chromizing is carried out in mixture containing the following components, mass-%: metallic chromium, 0.8-12; ammonia chloride, 0.008-0.16; the remainder being corundum. In particular cases, case-hardening is carried out in solid carburizer at temperature of 900-1000°C continued for 90-240 min and chromizing is carried out at temperature of 900-950°C for 60-240 min.
EFFECT: increased saturating capacity; reduced duration of process; enhanced wear resistance and corrosion resistance of steel parts.
2 cl, 1 tbl,, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD AND COMPOSITION FOR BOROCHROME PLATING OF STEEL PRODUCTS IN FLUIDIZED BED | 1996 |
|
RU2157859C2 |
METHOD FOR THERMAL DIFFUSION CHROMIUM PLATING OF PARTS MADE OF STEEL OR IRON-BASED ALLOYS WITH ADDITION OF EMITTER TO SATURATING POWDER MIXTURE | 2022 |
|
RU2792514C1 |
STRENGTHENING METHOD OF STEEL PARTS | 2008 |
|
RU2381299C1 |
METHOD OF THERMAL DIFFUSION CHROMIUM PLATING OF STEELS AND IRON-BASED ALLOYS USING CUMULATIVE GRIDS | 2023 |
|
RU2794655C1 |
PART CARBON CHROME-PLATING METHOD | 1994 |
|
RU2057201C1 |
COMPOSITION FOR CHROMIUM PLATING OF STEEL PRODUCTS | 0 |
|
SU1137112A1 |
METHOD OF CHROMIZING METAL MATERIALS IN FLUIDIZED BED | 2002 |
|
RU2212470C1 |
CHROMIUM-PLATING METHOD OF STEEL PRODUCTS IN MUFFLE FURNACES WITH AIR ATMOSPHERE | 2008 |
|
RU2378413C2 |
METHOD FOR DIFFUSION CHROME-PLATING OF STEEL PRODUCTS IN FLUIDIZED BED | 2002 |
|
RU2209847C1 |
METHOD OF CHEMICAL-THERMAL WORKING OF HARD ALLOY TOOL | 1991 |
|
RU2009025C1 |
Authors
Dates
2006-10-20—Published
2004-05-12—Filed