FIELD: polymeric materials. SUBSTANCE: polymeric composition has, wt. -%: novolacs phenolformaldehyde resin, 25.89-43.2; urotropin, 4.5-6.6; wood flour, 18.21-43.23; ocher, 5.87-36.6; hardening accelerating agent, 0.5-4.0; and lubricant, 0.6-2.0. Composition is rolled on rollers at working roller temperature 70-90 C and at no-load roller temperature 110-130 C. Rolled material is crushed and ground. Heat stability of composition is 191.7-221 C. EFFECT: enhanced dielectric property and heat stability. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERIC COMPOSITION | 1996 |
|
RU2098438C1 |
POLYMERIC COMPOSITION | 1995 |
|
RU2100390C1 |
POLYMERIC COMPOSITION FOR ANTIFRICTION MATERIAL | 1996 |
|
RU2126429C1 |
ELECTOINSULATION POLYMER COMPOSITION FOR STAMPED PLATE | 1993 |
|
RU2061716C1 |
POLYMER COMPOSITION | 2010 |
|
RU2428442C1 |
POLYMER COMPOSITION | 1992 |
|
RU2005746C1 |
POLYMERIC PRESS-COMPOSITION | 0 |
|
SU852911A1 |
POLYMERIC COMPOSITION | 1994 |
|
RU2076885C1 |
POLYMERIC CASTING COMPOSITION | 2003 |
|
RU2250913C1 |
COMPOSITION FOR PREPARING PRESSING COMPOUND | 2000 |
|
RU2198189C2 |
Authors
Dates
1997-04-27—Published
1995-05-12—Filed