FIELD: production of motor oil. SUBSTANCE: proposed additive is prepared by cation polymerization of vinylbutyl ether which is carried out at 20-50 C in the medium of solvent. The process takes place in the presence of aluminium sesquiethyl chloride, its mass ratio to monomer being 0.3-0.5:100. Hydrocarbon of $$$ fraction is used as mentioned above solvent. Said solvent may additionally comprise mineral oil, its mass ratio to hydrocarbon is (5: 95)-(99:1). EFFECT: improved efficiency of the method. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
VULCANIZABLE CIS-1,4-BUTADIENE RUBBER BASED COMPOSITION | 1998 |
|
RU2154656C2 |
METHOD OF SYNTHESIS OF POLYISOBUTYLENE | 1998 |
|
RU2148590C1 |
METHOD OF PREPARING THICKENING AGENT | 2000 |
|
RU2194720C2 |
METHOD FOR PRODUCTION OF OIL-FILLED BUTADIENE/STYRENE THERMOELASTOLAYERS | 2000 |
|
RU2163912C1 |
METHOD OF PREPARING 1,2-POLYBUTADIENE | 1998 |
|
RU2134697C1 |
PROCESS FOR PREPARING LOW MOLECULAR WEIGHT 1,2-POLYBUTADIENE | 1995 |
|
RU2082722C1 |
POLYISOBUTYLENE PRODUCTION PROCESS | 1998 |
|
RU2130948C1 |
METHOD OF SYNTHESIS OF BUTADIENE-STYRENE RUBBER | 2001 |
|
RU2200740C1 |
METHOD FOR PRODUCING SYNTHETIC RUBBER | 2005 |
|
RU2288235C1 |
METHOD OF PREPARATION OF CIS-1,4,POLYBUTADIENE | 1995 |
|
RU2087489C1 |
Authors
Dates
1997-04-27—Published
1994-10-12—Filed