FIELD: manufacture of building materials. SUBSTANCE: when fabricating bulk structures of all- building destination (for example, floors or coatings), concrete coating 4-5 h after it has been shaped is covered with aqueous suspension of expanding additive with water to solids ratio 4-6 and then coating is aged for 8-10 h and leveled. EFFECT: improved quality of surface. 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| SEAMLESS POURED-IN-PLACE CONCRETE FLOOR | 1998 | 
 | RU2137730C1 | 
| METHOD OF MANUFACTURING HIGH-STRENGTH CELLULAR CONCRETE | 1998 | 
 | RU2133722C1 | 
| METHOD OF MAKING THE CONCRETE ARTICLES WITH AN OPEN STRUCTURE | 1992 | 
 | RU2046706C1 | 
| METHOD OF CONCRETING OF CONSTRUCTIONS AND PRODUCTS | 1990 | 
 | SU1812770A1 | 
| METHOD OF TREATMENT OF SETTING HIGHWAY COVERING CONCRETE | 0 | 
 | SU1719381A1 | 
| APPARATUS FOR FINISHING THE SURFACE OF FERROCONCRETE ARTICLES | 0 | 
 | SU1021625A1 | 
| METHOD OF MANUFACTURE OF REINFORCED CONCRETE MULTICAVITY ARTICLES | 1996 | 
 | RU2101170C1 | 
| LUBRICANT FOR METAL MOULDS | 1991 | 
 | RU2035300C1 | 
| METHOD FOR CAST-IN-SITU CEMENT CONCRETE COVERING ERECTION | 0 | 
 | SU1825834A1 | 
| METHOD OF ELECTRIC HEATING OF CONCRETE MIX | 1991 | 
 | RU2017610C1 | 
Authors
Dates
1997-05-10—Published
1995-02-21—Filed