FIELD: simulated natural materials. SUBSTANCE: 50-% aqueous dispersion of butylacrylate/methylmetacrylate/metacrylic acid/glycidylmetacrylate copolymer is characterized with monomer weight ratio (62-64):(31-33):(3.3-5.3): (0.45-0.95), respectively. 8- 10 parts of kaolin is mixed with 0.2-0.4 parts of aniline dyestuff and 45-50 parts of water at 80-100 C. Obtained mixture is cooled to 25 C, combined with 100 parts of above-indicated suspension to produce composition appropriate to be used for impregnating textile back followed by drying at 100-140 C. Characteristics of polyamide fiber material with textile back: longitudinal stiffness 10 cN, friction coefficient 0.12, resistance to repeated bent at 20 C 22000 cycles, light resistance 5 points, and coating weight increment 20-5 g/sq.m. EFFECT: improved user's quality. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
WATER-SOLUBLE CROSS-LINKABLE PROTECTIVE COLLOIDS, METHOD OF PREPARING AQUEOUS DISPERSIONS OF POLYMERS STABILIZED BY PROTECTIVE COLLOIDS, AQUEOUS POLYMER DISPERSIONS, AND POLYMER POWDER COMPOSITIONS SUITABLE FOR REDISPERSING IN WATER | 1997 |
|
RU2171813C2 |
0 |
|
SU524525A3 | |
METHOD FOR PREPARING ACRYLIC COPOLYMER AQUEOUS DISPERSION FOR PRESSURE-SENSITIVE GLUES | 2006 |
|
RU2315062C1 |
METHOD FOR PREPARING STYRENE-ACRYLIC COPOLYMERS AQUEOUS DISPERSIONS | 2004 |
|
RU2260602C1 |
METHOD OF PRODUCING DIALLYLPHTHALATE, BUTYLACRYLATE AND METHYLMETHACRYLATE COPOLYMERS | 0 |
|
SU789530A1 |
METHOD FOR PRODUCING FLUORINE-CONTAINING POLYMER, WATER DISPERSION LIQUID AND COMPOSITION OF FLUORINE-CONTAINING POLYMER | 2020 |
|
RU2814921C2 |
BINDER FOR PREPARING GLUED NON-WOVEN CLOTH | 1991 |
|
RU2026322C1 |
AQUEOUS STYRENE-ACRYLIC DISPERSION AND PREPARATION METHOD THEREOF | 2014 |
|
RU2568440C1 |
BINDING MATERIAL | 0 |
|
SU1821504A1 |
LATEX SYSTEM AND METHOD OF PREPARATION THEREOF | 1995 |
|
RU2156775C2 |
Authors
Dates
1997-06-10—Published
1990-04-09—Filed