FIELD: polymeric materials. SUBSTANCE: composition has the following components, wt.-%: polyphenylene oxide, polystyrene or their mixture 20-60; polypropylene 5-66; grafted copolymer of styrene and polypropylene (styrene content is 30-45 wt.-%), and block-copolymer of vinylaromatic monomer and coupled diene 4-10. Composition is used as plastics exhibiting high heat-stability and stretching strength at increased temperatures. EFFECT: enhanced quality of composition. 5 cl, 6 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| THERMOPLASTIC COMPOSITION | 1991 |
|
RU2081888C1 |
| POLYMERIC COMPOSITION | 1996 |
|
RU2171821C2 |
| IMPACT-RESISTANT COMPOSITION | 1993 |
|
RU2107079C1 |
| THERMOPLASTIC COMPOSITION | 1991 |
|
RU2091411C1 |
| METHOD FOR PREPARING POLYPROPYLENE GRAFTED COPOLYMERS CONTAINING ANHYDRIDE GROUPS | 1998 |
|
RU2211844C2 |
| THERMOELASTIC ELASTOMER COMPOSITION BEING DYNAMICALLY PARTIALLY HARDENED BY ORGANIC PEROXIDES | 1991 |
|
RU2083612C1 |
| POLYMER COMPOSITION AND METHOD FOR RETARDING DEPOLYMERIZATION OF POLYMETHYLMETHACRYLATE | 1997 |
|
RU2198902C2 |
| GRAFTED OLEFIN POLYMER AND METHOD FOR ITS PRODUCTION | 1990 |
|
RU2090574C1 |
| APPLICATION OF NITROGEN OXIDE FOR REDUCING REACTOR STOPPAGE IN GRAFTING COPOLYMERIZATION OF POLYPROPYLENE | 1998 |
|
RU2216550C2 |
| ELASTIC PLASTIC COMPOSITION AND METHOD FOR ITS PRODUCTION | 1988 |
|
RU2074868C1 |
Authors
Dates
1997-06-20—Published
1991-03-25—Filed