FIELD: powder metallurgy, in particular, production of titanium-nickel alloy close to equivalent composition of titanium nickeline possessing form memory and high damping effect. SUBSTANCE: method involves mixing titanium and nickel powders taken in the ratio of 55-57% by weight of nickel and titanium the balance; subjecting obtained mixture to cyclic diffusion thermal treatment, with mixture being supplied in free flowing state. Thermal treatment is initiated with heating to temperature of 600 C with further elevating of temperature by 50 C in each subsequent cycle till temperature of 1,050 C is reached, with holding time of 1 hour being provided beginning from 950 C under vacuum of 10-3 Pa. Titanium carbide is added into basic mixture in an amount of 0.5% by weight of basic mixture. EFFECT: increased efficiency, simplified method and improved quality of produced alloy. 2 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING TITANIUM-NICKEL ALLOY OF EUTECTIC COMPOSITION | 0 |
|
SU1482772A1 |
METHOD OF PRODUCING POROUS TITANIUM NICKELID OXIDE | 2010 |
|
RU2522257C2 |
METHOD OF PRODUCING POWDER ALLOYS OF SPHERICAL SHAPE BASED ON TITANIUM NICKELIDE FOR USE IN ADDITIVE TECHNOLOGIES | 2021 |
|
RU2779571C2 |
METHOD FOR PRODUCING A PRODUCT FROM A COMPOSITE MATERIAL BASED ON TUNGSTEN AND TITANIUM CARBIDES (VERSIONS) | 2021 |
|
RU2775048C1 |
POWDER WIRE FOR DURABLE FACING | 2003 |
|
RU2259266C2 |
POWDER WIRE FOR SURFACING | 2003 |
|
RU2254219C1 |
METHOD FOR PREPARING COMPLEX TITANIUM-BASED CARBIDE POWDER | 0 |
|
SU1678534A1 |
POWDER MATERIAL TREATMENT METHOD | 1994 |
|
RU2082556C1 |
METHOD OF PRODUCING ALLOYED POWDERS IN VIBROFLUIDISED BED | 2015 |
|
RU2606358C2 |
PROCEDURE FOR PRODUCTION OF POROUS TITANIUM NICKELIDE | 2008 |
|
RU2394112C2 |
Authors
Dates
1997-06-27—Published
1993-08-16—Filed