FIELD: chemical industry. SUBSTANCE: invention describes method of opening molybdenum and recovery of manganese from pyrolysite by combined treatment thereof in sulfuric acid solutions. Treatment is carried out in autoclave at 150-200 C and molar ratio of 1:4-8 for 2-6 hr in one stage at initial sulfuric acid concentration of 10-25%. EFFECT: more efficient opening method. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PROCESSING SULFIDE POLYMETALLIC MATERIALS | 1997 |
|
RU2119962C1 |
| METHOD OF EXTRACTING LEAD AND PHYSICO-CHEMICAL MODIFICATION OF SILVER | 1995 |
|
RU2086680C1 |
| METHOD OF PREPARING γ--MODIFICATION OF MANGANESE DIOXIDE | 1996 |
|
RU2115769C1 |
| METHOD OF SYNTHESIS OF MANGANESE DIOXIDE OF GAMMA-MODIFICATION | 1997 |
|
RU2149832C1 |
| METHOD OF CONCENTRATING SULFIDE SIDERITE-CONTAINING ORES | 1996 |
|
RU2123885C1 |
| PROCESS FOR RECOVERY OF COPPER, NICKEL AND COBALT FROM ARSENIC-CONTAINING AMMONIA-CARBONATE SOLUTIONS | 1995 |
|
RU2082782C1 |
| METHOD FOR FLOTATION OF SULFIDE COPPER-NICKEL ORES | 1995 |
|
RU2097141C1 |
| METHOD OF ISOLATING TRIBUTYL PHOSPHATE FROM AQUEOUS SOLUTIONS | 1997 |
|
RU2123976C1 |
| METHOD OF REMOVING HEAVY NONFERROUS METALS FROM AMMONIUM MOLYBDATE SOLUTION | 1996 |
|
RU2116969C1 |
| METHOD OF SULFIDE COPPER-NICKEL ORE FLOTATION | 1994 |
|
RU2067030C1 |
Authors
Dates
1997-06-27—Published
1995-01-11—Filed