FIELD: abrasive materials. SUBSTANCE: glass is mixed with 10.5-28.0% blowing agent, heated at temperature 765-960 C and then cooled to room temperature. Abrasive washing of fabric on washing machine is performed, glass foam blocks being installed on blades of machine. EFFECT: improved manufacture procedure. 26 cl
Title | Year | Author | Number |
---|---|---|---|
FOAMING MIXTURE AND A METHOD OF PRODUCTION OF A MODULAR FOAMED GLASS WITH THE MIXTURE USE | 2003 |
|
RU2265582C2 |
CHARGE FOR PRODUCING FOAMED GLASS | 2017 |
|
RU2684654C2 |
METHOD OF PREPARING BLEND FOR FABRICATING GLASS FOAM | 2003 |
|
RU2255058C1 |
METHOD OF PREPARING RAW MIX FOR FABRICATING GLASS FOAM | 2003 |
|
RU2255057C1 |
METHOD OF PRODUCING FOAMED GLASS | 2010 |
|
RU2459769C2 |
METHOD OF PRODUCING FOAMED GLASS | 2019 |
|
RU2701951C1 |
METHOD FOR PRODUCTION OF GRANULATED FOAMED GLASS | 2018 |
|
RU2698388C1 |
LIQUID OR SOLID DETERGENT COMPOSITION WITH CONTROLLED FOAMING FOR WASHING FABRIC, METHOD FOR WASHING FABRIC, WASHING PARTICLES | 1991 |
|
RU2112784C1 |
METHOD OF PRODUCING FOAMED GLASS AND FOAMED GLASS COMPOSITION | 2010 |
|
RU2417958C1 |
METHOD FOR PRODUCTION OF FOAM GLASS | 2008 |
|
RU2351554C1 |
Authors
Dates
1997-08-20—Published
1993-05-12—Filed