FIELD: protection of underground pipelines. SUBSTANCE: adhesion composition comprises, mas.p.: high pressure polyethylene, 100; talc, 26; titanium dioxide, 4.3; technical carbon, 0.02; antioxidant, 0.1; ethylene-vinyl acetate copolymer (content of vinyl acetate groups in it is 16-17 mass %), 87.0-130.3. 2,2′-methylene-bis/6-tert-butyl-4-methyl phenol/ is used as mentioned above antioxidant. Composition is applied on metal, the process is carried out at 160-200 C within 2 min and it is followed by jointing. EFFECT: improved quality of desired product. 7 tbl
Title | Year | Author | Number |
---|---|---|---|
ADHESION COMPOSITION | 1993 |
|
RU2068867C1 |
PRIMING COMPOSITION | 1996 |
|
RU2099374C1 |
INSULATION COATING FOR PROTECTION PIPES AGAINST UNDERGROUND CORROSION | 1995 |
|
RU2087507C1 |
ADHESION COMPOSITE | 2001 |
|
RU2186082C1 |
PROCESS OF MANUFACTURE OF PROTECTIVE COAT OF HIGH-VOLTAGE INSULATOR | 1993 |
|
RU2037218C1 |
METHOD OF PRODUCTION OF THE ADHESIVE COMPOSITION | 2005 |
|
RU2311435C2 |
PRIMING COMPOSITION | 1995 |
|
RU2089582C1 |
COMPOSITION FOR MAKING ADHESIVE MELTS AND METHOD OF PREPARATION THEREOF | 1998 |
|
RU2143451C1 |
METHOD OF PREPARING POWDER POLYMER COATING | 2002 |
|
RU2220998C1 |
METHOD FOR MANUFACTURING POLYETHYLENE ADHESIVE COMPOSITION FOR ANTI-CORROSIVE DECORATIVE COATINGS AND POLYETHYLENE ADHESIVE COMPOSITION FOR ANTI-CORROSIVE DECORATIVE COATINGS OBTAINED BY THIS METHOD | 2022 |
|
RU2810787C1 |
Authors
Dates
1997-09-10—Published
1993-03-02—Filed