FIELD: production of blue aluminium-cobalt pigment which may be used in paint and varnish industry, in artistic and restoration works; production of paint for ceramics. SUBSTANCE: method involves mixing of compounds of cobalt and aluminium, mechanical activation of mixture in centrifugal mill and calcination. Co3O4 and aluminium hydroxide having pseudobemite structure or powder of metal aluminium are used as origin components. Activation is carried out at power strength 10-50 Wt/g, it is followed by grinding of caked agglomerates prepared by calcination, the process takes place till average size of particles is 0.5-1.0 mcm. Pigment comprises, mas.%: CoO, 22-25; Al2O3, the balance. EFFECT: improved properties. 4 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING HEAT-RESISTANT INORGANIC PIGMENTS | 1997 |
|
RU2114886C1 |
METHOD OF PRODUCING ALUMINATE | 1996 |
|
RU2108292C1 |
METHOD OF ALKALINE-EARTH METAL ALUMINOSILICATE PRODUCING | 1993 |
|
RU2078037C1 |
method of preparing thermoelectric material | 1996 |
|
RU2118669C1 |
METHOD OF PRODUCING OF LITHIUM PENTALUMINATE LiAlO | 1992 |
|
RU2034784C1 |
PROCESS FOR MANUFACTURING OF FERROUS IRON-BASED DOUBLE METALLIC OXIDES | 1990 |
|
RU2008264C1 |
AMMONIA OXIDATION CATALYST | 1996 |
|
RU2100068C1 |
METHOD FOR PREPARATION OF MIXTURE FOR HARD ALLOYS BASED ON TUNGSTEN CARBIDE | 1996 |
|
RU2120840C1 |
SENSITIVE ELEMENT OF PARTIAL PRESSURE TRANSDUCER OF NO 002 OF GAS MIXTURES | 1992 |
|
RU2049993C1 |
METHOD OF OBTAINING AMORPHOUS ALUMINUM HYDROXIDE | 1985 |
|
RU1277552C |
Authors
Dates
1997-09-20—Published
1995-10-12—Filed