FIELD: metallurgy. SUBSTANCE: method involves multiple heating carbon tool steel above Ac1 by 40-80 C at the rate 4-8 C/s, cooling at cycle below Ac1 to 250-300 C at the rate 1-7 C/s and tempering at 160-240 C. Method can be used in machine engineering. EFFECT: improved method of steel working. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF THERMOCYCLIC TREATMENT OF TOOL STEEL | 1998 |
|
RU2131469C1 |
METHOD OF THERMOCYCLIC TREATMENT OF HIGHCHROMIUM TOOL STEEL FOR SECONDARY HARDNESS | 2000 |
|
RU2192485C2 |
METHOD OF IMPROVING HEAT TREATMENT OF STEEL | 1998 |
|
RU2131932C1 |
TOOL STEELS THERMAL PROCESSING METHOD | 1991 |
|
RU2017838C1 |
METHOD OF RECONDITIONING PISTON PINS MADE OF STEEL CEMENT GRADES OF AUTOMOTIVE ENGINES | 1996 |
|
RU2122588C1 |
METHOD FOR THERMAL TREATMENT OF STEEL CONSTRUCTIONS WITH STRESS CONCENTRATORS | 2001 |
|
RU2204615C2 |
METHOD FOR SECONDARY HARDNESS THERMAL TREATMENT OF HIGH-CHROMIUM TOOL STEEL | 2001 |
|
RU2200201C2 |
CAST PRESSED STEEL | 1996 |
|
RU2095460C1 |
METHOD OF HARDENING OBJECTS OF CARBON, ALLOYED, HIGH-ALLOY, AND QUICK- CUTTING STEELS, AND HARD ALLOYS | 1996 |
|
RU2100456C1 |
Authors
Dates
1997-09-20—Published
1995-12-01—Filed