FIELD: metallurgy, in particular, repair and manufacture of annealing unit roller. SUBSTANCE: roller has pins provided with inner layer of austenitic stainless steel and outer layer of martensitic stainless steel. Thickness of outer layer does not exceed 0.5 of total thickness of hollow pin wall. Alloy , which may be used as material for inner layer, contains, % by weight: carbon 0.01-0.12; manganese 0.1-2.0; chromium 16.0-20.0; silicon 0.01-0.08; nickel 8.0-11.0; iron the balance. Alloy used as material for outer layer contains, % by weight: carbon 0.09-0.25; silicon 0.10-0.80; manganese 0.10-0.80; chromium 12.00-14.00; nickel 0.01-0.60; iron the balance. EFFECT: increased efficiency, simplified construction and enhanced reliability in operation. 4 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ROLLERS REPAIR | 1996 |
|
RU2096156C1 |
ALLOY COMPOSITION | 1996 |
|
RU2104324C1 |
BEARING ROLLER | 2002 |
|
RU2221204C1 |
SHROUDING RING OF ROLLER AND PROCESS OF ITS MANUFACTURE | 1997 |
|
RU2124962C1 |
ALLOY COMPOSITION | 1998 |
|
RU2131945C1 |
ROLLING ROLL | 1995 |
|
RU2087218C1 |
ALLOY FOR ELECTROSLAG WELDING-ON OF CAST IRON ROLLING ROLLS | 2001 |
|
RU2197552C1 |
CORROSION-RESISTANT STEEL OF MARTENSITE CLASS AND ITEM MADE OUT OF THIS STEEL | 2008 |
|
RU2369657C1 |
HIGH-STRENGTH CORROSION-RESISTANT STEEL | 2004 |
|
RU2271402C1 |
PRODUCTION OF STEEL SHEETS OF HIGHER WEAR RESISTANCE | 2016 |
|
RU2625861C1 |
Authors
Dates
1997-10-20—Published
1996-06-03—Filed