FIELD: polymeric composition. SUBSTANCE: method involves applying three layers at 15-30 min interval between each layer of polymeric composition that has, p. p.: methylmethacrylate 100; polybutylmethacrylate 10-70; butylmethacrylate 5-60; polyisocyanate 10-40; dimethylaniline 0.05-2.00; divinylbenzene 0.1-10; benzoyl peroxide 0.1-10.0; perchlorovinyl resin 0.5-25.0; diethanolamine maleinate 0.01-0.50, and amine 0.01-1.00. For median layer composition has additionally silicon carbide. Coating hardening time is 3-4 h, complete hardening - for 10 days. Composition is used for cathode protection in electrolysis bath for pure metal producing. EFFECT: improved method of isolation. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
CHEMICALLY STABLE POLYMERIC COMPOSITION FOR COATINGS | 1992 |
|
SU1831872A3 |
CHEMICALLY RESISTANT POLYMER COMPOSITION FOR COATINGS | 1992 |
|
SU1831871A3 |
WATER RESISTANCE AND CRACK-RESISTING POLYMER COMPOSITION | 1992 |
|
SU1831870A3 |
ACIDPROOF POLYMER COMPOSITION FOR COATINGS | 1991 |
|
SU1825510A3 |
HEAT-RESISTANT ANTIFOULING POLYMER COMPOSITION FOR COATINGS | 1992 |
|
RU2028347C1 |
POLYMERIZABLE COMPOSITE MATERIAL | 1996 |
|
RU2119515C1 |
POLYURETHANE COMPOSITION FOR COATINGS | 2001 |
|
RU2188838C1 |
POLYURETHANE COMPOSITION FOR COATING | 2002 |
|
RU2216566C1 |
COMPOSITION FOR PROTECTIVE ANTICORROSIVE COATING | 2003 |
|
RU2258725C2 |
POLYMERIC COMPOSITION OF COLD SOLIDIFICATION FOR WATER PROOF COATINGS | 1991 |
|
SU1825511A3 |
Authors
Dates
1997-11-27—Published
1994-01-26—Filed