FIELD: production of anti-wear and antifriction materials; production of additives for oil compositions used in various engines. SUBSTANCE: fluoroplast-4 is affected by thermal destruction, the process is carried out at 480-540 C in stream of circulating gaseous products of thermal destruction which comprises 0.05-1 vol % of oxygen saturated by water or 0.1-5 vol % of air saturated by water. Thus prepared material as concentrated suspension comprising 1-85 mass % of polytetrafluoroethylene is fed into oil composition, the process is carried out till effective concentration of polytetrafluoroethylene is 0.1-20 mass %. EFFECT: higher efficiency; increased stability of oil suspension. 3 cl, 1 dwg, 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING NANODISPERSED FLUOROPLASTIC | 2012 |
|
RU2501815C1 |
ADDITIVE "F19" AND LUBRICATING MATERIAL CONTAINING THE LATTER | 2001 |
|
RU2195477C1 |
METHOD OF OBTAINING NANODISPERSIVE FLUOROORGANC MATERIAL | 2007 |
|
RU2341536C1 |
METHOD OF UTILIZING CARBOCHAIN THERMOPLASTICS TO PRODUCE FINE POWDER | 2001 |
|
RU2210577C2 |
LUBRICATING COMPOSITION | 2014 |
|
RU2570403C2 |
METHOD OF DECREASING VIBRATION ACTIVITY OF MECHANISMS | 1995 |
|
RU2084716C1 |
METHOD FOR PROCESSING POLYTETRAFLUORETHELEN | 0 |
|
SU1775419A1 |
METHOD OF MANUFACTURING FLUOROPLASTIC | 2007 |
|
RU2326128C1 |
METHOD OF PROCESSING POLYTETRAFLUOROETHYLENE | 2014 |
|
RU2561111C1 |
EQUIPMENT FOR POLYTETRAFLUOROETHYLENE PROCESSING | 0 |
|
SU1763210A1 |
Authors
Dates
1997-12-27—Published
1995-10-12—Filed