FIELD: polymer fibers. SUBSTANCE: polyacrylonitrile fiber with 1.5 wt. -% of carboxyl groups is treated with aqueous solution containing 8-15% hydrazine and 1-2% sodium hydroxide at 90-100 C for 120-150 min. EFFECT: acquired ion-exchange property. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING ION-EXCHANGE POLYACRYLONITRILE FIBER (OPTIONS) | 2004 |
|
RU2262557C1 |
CHEMISORPTION MATERIAL MANUFACTURE METHOD | 2002 |
|
RU2258716C2 |
METHOD OF PREPARING CARBON-CONTAINING OBJECTS | 1993 |
|
RU2070435C1 |
POLYAMPHOLITE FIBER CARBONACEOUS MATERIAL, METHOD OF PREPARING MATERIAL, AND ARRANGEMENT FOR CONTINUOUS ACTIVATION THEREOF | 1993 |
|
RU2070436C1 |
METHOD OF MANUFACTURING BUILDING PARTS AND RAW CERAMIC MASS FOR MANUFACTURING BUILDING PARTS | 1994 |
|
RU2100324C1 |
METHOD OF PREPARING CARBON MATERIAL | 1995 |
|
RU2093495C1 |
METHOD FOR PRODUCTION OF ANTICORROSION PIGMENT ON BASE OF ALUMINIUM TRIPHOSPHATE | 1995 |
|
RU2102420C1 |
METHOD OF OBTAINING ANION-EXCHANGE FIBRE MATERIAL, CAPABLE OF EXTRACTING CHROMIUM (VI) | 2008 |
|
RU2368711C1 |
METHOD FOR PRODUCTION OF METALLIC PLATINUM | 1995 |
|
RU2083704C1 |
METHOD OF TREATING SEDIMENTS FROM DOMESTIC OR INDUSTRIAL WASTE WATER | 1992 |
|
RU2070165C1 |
Authors
Dates
1998-01-20—Published
1996-06-28—Filed