FIELD: metallurgy. SUBSTANCE: cover has metal casting with refractory lining. Attached to internal concave surface of casting are at least two wavy metal strips. Lining is made from heat-resistant concrete with filler in the form of chopped steel wire. Filler content in periphery circular part of lining in the region of its contact with ladle lining amounts to 4-5-8% and in central part, 2-4%. Width of periphery circular part amounts to 0.05-0.15 of inner diameter of cover lining. EFFECT: higher stability of cover due to presence of filler in concrete and metal strips. 2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
LID FOR STEEL CASTING LADLE | 1998 |
|
RU2148473C1 |
METHOD FOR PREPARING POURING LADLE IN THE PROCESS OF CONTINUOUS STEEL CASTING | 1994 |
|
RU2025202C1 |
STEEL CASTING LADLE | 1995 |
|
RU2092279C1 |
STEEL TEEMING LADLE | 1996 |
|
RU2096129C1 |
STEEL CASTING LADLE | 1996 |
|
RU2095192C1 |
STEEL CASTING LADLE | 1998 |
|
RU2148474C1 |
ELECTRIC FURNACE FOR SMELTING OF SYNTHETIC SLAG | 1995 |
|
RU2096490C1 |
TUNDISH | 2000 |
|
RU2167030C1 |
STEEL-TEEMING LADLE LINING METHOD | 1998 |
|
RU2138366C1 |
STEEL CASTING LADLE | 1995 |
|
RU2083324C1 |
Authors
Dates
1998-02-10—Published
1996-07-02—Filed