FIELD: tyre and rubber industry. SUBSTANCE: material is fabricated from alternating polyisoprene rubber layers and reinforcing textile cord of alifatic polyamide with strength 85- 90 N/tex impregnated with latex-resorcin-formaldehyde formulation. Cord is impregnated for 7-15 s and dried for 7-15 min at 125-150 C. Material is thermally treated at 190-230 C in two steps each lasting 20-30 s. Material is characterized by strength of join with rubber 102-131 N at 23 C and 81-101 N at 120 C. EFFECT: improved performance characteristic s. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR TREATMENT OF POLYESTER CORD | 1993 |
|
RU2054058C1 |
ARAMIDE CORD THREAD | 2012 |
|
RU2495970C1 |
RUBBER-CORD COMPOSITE MATERIAL | 2006 |
|
RU2305037C1 |
POLYAMIDE CORD FABRIC FOR MULTILAYER TIRE CARCASS | 2020 |
|
RU2731702C1 |
CORD HYBRID FABRIC FOR MULTILAYER TIRE CARCASS | 2020 |
|
RU2729526C1 |
METHOD OF HEAT TREATMENT OF ANIDE CORD | 2007 |
|
RU2373308C2 |
CORD THREAD | 2009 |
|
RU2391452C1 |
VULCANIZABLE RUBBER MIX FOR FIXING TO KAPRON CORD | 1987 |
|
RU2016007C1 |
METHOD OF COATING SYNTHETIC ROPE | 2014 |
|
RU2553963C1 |
METHOD OF ARAMID CORD TREATMENT | 2006 |
|
RU2330132C2 |
Authors
Dates
1998-04-27—Published
1996-03-14—Filed