FIELD: polymers. SUBSTANCE: high-strength high-module fibers and threads that are used for plastics reinforcement, in rubber-technical articles, heat-insulating and protective materials are obtained from anisotropic solution based on aromatic copolyamide containing aromatic copolyamide of the formula given in description where m = 0.95-0.75; n = 0.05-0.25 where X - H or Cl; Y - Cl, at logarithmic viscosity 2.96-6.08 dl/g and sulfuric acid (concentration is 98.0-99.8%). Copolyamide concentration in solution is 11-20 wt. -%. Formed articles exhibit the following properties: linear density is 29.8-33.4 tex, not less; oxygen index is 33-46; rupture strength is 35 sN/tex, not less; rupture elongation is 3.2-15%; initial elasticity module is 3250 kgf/mm2 and thermic stability is 90-118%. EFFECT: improved quality and properties of product. 2 cl, 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| SOLUTION FOR MANUFACTURING POLYAMIDE FILAMENTS | 1993 |
|
RU2063487C1 |
| ANISOTROPIC SOLUTION FOR MOLDING THREAD AND THREAD WHICH IS PREPARED OF SAID SOLUTION | 1993 |
|
RU2045586C1 |
| AROMATIC-BASE COPOLYAMIDE FORMED ARTICLE | 2000 |
|
RU2167961C1 |
| METHOD OF MANUFACTURING THREADS BASED ON AROMATIC COPOLYAMIDES | 2000 |
|
RU2168567C1 |
| SPINNING SOLUTION COMPOSITION AND THREADS FORMED THEREFROM | 1995 |
|
RU2146729C1 |
| METHOD OF PRODUCING AROMATIC COPOLYAMIDES (VERSIONS) AND HIGH-STRENGTH HIGH-MODULUS FIBRES BASED THEREON | 2011 |
|
RU2469052C1 |
| METHOD FOR DYEING AROMATIC POLYAMIDE FIBERS | 1992 |
|
RU2010896C1 |
| FIBER OR FILM MOLDING COMPOSITION | 2002 |
|
RU2215833C1 |
| COMPOSITE HIGH-STRENGTH, HIGH-MODULUS HEAT-RESISTANT FIBRE MADE FROM HETEROCYCLIC AROMATIC COPOLYAMIDE AND METHOD FOR PRODUCTION THEREOF (VERSIONS) | 2011 |
|
RU2487969C1 |
| ARAMIDE FIBER DYEING METHOD | 2001 |
|
RU2210649C2 |
Authors
Dates
1998-05-27—Published
1996-09-26—Filed