FIELD: building materials. SUBSTANCE: fibroconcrete mixture involving cement M400, mineral fiber (kaolin or basalt fiber), sand and water has additionally polyvinyl alcohol and building gypsum at the following ratio of components, wt. -%: cement M44, 20-25; indicated mineral fiber, 2-4; sand, 50-55; polyvinyl alcohol, 1-2 (by dry residue); building gypsum, 4-6; and water, the balance. Granules of polyvinyl alcohol are dissolved preliminary in water to homogeneous mass at 80-90 C for 50-70 min and solution is cooled to environment air point. Components are mixed in mixer of forced type. EFFECT: improved quality of mixture. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| POLYMER CONCRETE MIX | 1996 |
|
RU2117644C1 |
| CONCRETE MIXTURE | 2011 |
|
RU2480428C1 |
| BINDER | 1991 |
|
RU2047576C1 |
| AUTOCLAVED AERATED CONCRETE PRODUCT, METHOD OF ITS MANUFACTURE, MIXTURE FOR ITS MANUFACTURE AND METHOD OF MANUFACTURE OF MIXTURE | 2018 |
|
RU2681166C1 |
| FIBRE-CONCRETE MIXTURE | 2010 |
|
RU2423331C1 |
| CONCRETE MIXTURE | 2005 |
|
RU2288198C1 |
| RAW MATERIAL MIXTURE FOR HIGH-STRENGTH FIBRE-REINFORCED CONCRETE | 2014 |
|
RU2569140C1 |
| COMPOSITION FOR MANUFACTURE OF BUILDING MATERIALS | 2000 |
|
RU2233254C2 |
| MODIFIED POLYMER-CEMENT COMPOSITE MATERIAL FOR 3D PRINTING | 2017 |
|
RU2662838C1 |
| COMPLEX ADMIXTURE FOR CONCRETE MIX, AND METHOD FOR ITS MANUFACTURE | 2013 |
|
RU2545226C1 |
Authors
Dates
1998-06-27—Published
1995-09-19—Filed