FIELD: production of abrasive materials and tools. SUBSTANCE: method includes mixing of hexagonal boron nitride, magnesium and hydrazine chloride in the amount of 38-63 wt.% of the mixture; placement into high-pressure chamber; treatment with high pressure and temperature for the time enough for formation of borozon BN. Yield of borozon BN with grain size above 100 mcm amounts to 25.2-33.5 wt% or 1.6-2.75 carats for one press-sintering. EFFECT: higher efficiency. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ELEVATED-STRENGTH CUBIC BORON NITRIDE PREPARATION METHOD | 2002 |
|
RU2229434C2 |
METHOD OF PREPARING CUBICALLY STRUCTURED SUPERHARD MATERIALS | 1999 |
|
RU2159736C1 |
METHOD OF PRODUCING POLYCRYSTALLINE COMPOSITE MATERIAL | 2011 |
|
RU2525005C2 |
METHOD FOR PRODUCING CUBIC CRYSTALS OF BORON NITRIDE | 2002 |
|
RU2216611C1 |
METHOD OF PRODUCTION OF SUPERHARD COMPOSITE MATERIAL ON BASE OF CUBIC BORON NITRIDE FOR CUTTING AND COMPOSITE MATERIAL | 1999 |
|
RU2147972C1 |
METHOD OF MAKING POLYCRYSTALLINE MATERIAL BASED ON CUBIC BORON NITRIDE CONTAINING DIAMONDS | 2011 |
|
RU2484888C1 |
METHOD OF MANUFACTURING PRODUCTS FROM SUPERHARD COMPOSITE MATERIALS | 1994 |
|
RU2098388C1 |
METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD | 2004 |
|
RU2284247C2 |
COATING FOR ABRASIVE POWDERS | 0 |
|
SU1087495A1 |
METHOD OF PRODUCING POLYCRYSTALLINE CUBIC BORON NITRIDE | 2009 |
|
RU2412111C1 |
Authors
Dates
1998-07-27—Published
1993-08-19—Filed