FIELD: manufacture of abrasive materials. SUBSTANCE: graphite fluoride C2F or C2F•y ClF3 is reduced with liquid ammonia. Solid reaction products are decomposed at 250-400 C. Instead of ClF3 non-metal oxides, mineral acids or organic compounds are used. The claimed method is carried out at low pressure and temperatures, and technology is simplified. EFFECT: more efficient preparation method. 2 ex, 1 tbl