FIELD: hydrodynamic mixers. SUBSTANCE: each of two outlet nozzles is directed opposite to each other and made with length-width ratio of (4-6):1 with a distance between nozzles equalling 1.5-2.5 widths of nozzles and angle of nozzle exterior chamfer equals to 30-60 deg. EFFECT: production of oil-extended rubbers with high-degree of uniformity in distribution of oil in rubber. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SEPARATING RUBBERS PRODUCED BY EMULSION POLYMERIZATION AND DEVICE FOR FLOCCULATION | 1997 |
|
RU2146265C1 |
METHOD OF ISOLATING SYNTHETIC EMULSION RUBBERS | 1997 |
|
RU2144542C1 |
PROCESS FOR RECOVERING OIL-FILLED BUTADIENE-(α-METHYL) STURENE RUBBER | 1993 |
|
RU2067590C1 |
PROCESS FOR RECOVERY OF OIL-FILLED BUTADIENE-(α-METHYL) STYRENE RUBBER | 1993 |
|
RU2067591C1 |
METHOD OF ISOLATION OF OIL-FILLED BUTADIENE-(α-METHYL)-STYRENE RUBBER | 1993 |
|
RU2064939C1 |
PROCESS FOR RECOVERY OF BUTADIENE-(α-METHYL)STYRENE RUBBER | 1994 |
|
RU2067592C1 |
FILLED BUTADIENE-STYRENE RUBBER PRODUCTION PROCESS | 2005 |
|
RU2289590C1 |
METHOD FOR PRODUCING BUTADIENE-STYRENE RUBBER | 2017 |
|
RU2660084C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2005 |
|
RU2291159C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2006 |
|
RU2291161C1 |
Authors
Dates
1998-08-10—Published
1996-11-12—Filed