FIELD: coatings. SUBSTANCE: method involves raising dust priming layer on article and intermediate layer containing, wt.-%: basic external metal 80-98; ground coat 1.0-19.0, and flux 1-19. Then external coating is applied on an intermediate layer followed by thermic treatment in nonoxidative atmosphere at priming layer melting point. EFFECT: increased coating thickness, enhanced adhesion and cohesion strength of coating. 1 ex
Title | Year | Author | Number |
---|---|---|---|
POLYUREA URETHANE SPRAYED MASTIC FOR OBTAINING THICK-LAYERED ANTICORROSION COATING | 2013 |
|
RU2531191C1 |
LIQUID HYDROXYLAMINE CURING AGENT FOR ISOCYANATE PREPOLYMERS FOR PRODUCING SPRAYED POLYUREA-URETHANE COATINGS | 2013 |
|
RU2522427C1 |
COMPLEX ANTI-CORROSION POLYUREA-URETHANE COATING | 2010 |
|
RU2428443C1 |
METHOD FOR RESTORATION OF WORN SURFACES OF BLOCK JOURNALS OF WHEEL SET AXLES IN ROLLING STOCK AND TRACK MACHINES | 2008 |
|
RU2380208C1 |
METHOD OF PROFILE RESTORATION OF BLADE BODY OF GAS TURBINE ENGINE | 2014 |
|
RU2556175C1 |
METHOD FOR MANUFACTURING OF ANTIFRICTION RECOVERY COATING AT STEEL PRODUCT (VERSIONS) | 2012 |
|
RU2532653C2 |
RESISTANCE SPOT WELDING METHOD | 2004 |
|
RU2270081C1 |
PHOSPHOTIZING PRIMER | 1997 |
|
RU2142970C1 |
METHOD OF PROTECTING BLADES AND NOZZLE ASSEMBLY OF GAS TURBINES | 2023 |
|
RU2818096C1 |
EXPLOSIVE EVAPORATION DEVICE | 1997 |
|
RU2140334C1 |
Authors
Dates
1998-10-10—Published
1997-09-26—Filed