FIELD: manufacture of tires and industrial rubber products. SUBSTANCE: hard rosin is modified by maleic anhydride and formaldehyde on heating in the presence of 0.02-0.05% based on weight of dimethylpolysiloxane rosin with viscosity of 200-400 sq m/s. Test resin samples make rubbers adhesive and make it possible to use resin based on tall hard rosin to replace pine gum rosin and rosin, grade EM-3. EFFECT: more efficient preparation method. 2 cl, 4 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RESIN FOR INCREASING ADHESIVENESS OF RUBBER MIXTURES | 2013 |
|
RU2559468C2 |
METHOD OF PRODUCING HYDROCARBON RESIN SINGER 10P | 2015 |
|
RU2640549C2 |
METHOD OF PREPARING COLOPHONY ETHERS | 1996 |
|
RU2119517C1 |
PROCESS FOR PREPARING MODIFIED CALOPHONY | 0 |
|
SU1039943A1 |
METHOD OF PREPARING COLOPHONY-TERPENE-MALEIC RESIN | 1994 |
|
RU2105781C1 |
COLOPHONY RESIN AND A METHOD FOR PREPARATION THEREOF | 2003 |
|
RU2229491C1 |
METHOD OF PREPARING MODIFIED COLOPHONY | 0 |
|
SU834064A1 |
METHOD OF CLARIFYING COLOPHONY AND ITS DERIVATIVES | 0 |
|
SU836065A1 |
METHOD OF DISPROPORTIONING MIXTURES OF FATTY AND RESIN ACIDS | 1997 |
|
RU2144527C1 |
0 |
|
SU551352A1 |
Authors
Dates
1999-05-10—Published
1997-03-25—Filed