FIELD: manufacture of constructional arbolite for industrial, agricultural and civil engineering. SUBSTANCE: arbolite mix comprises binder consisting of portland cement and additive, wood filler, calcium chloride and water contains, and as binder additive, sand in amount of 11-24 wt % at feldspar to quartz ratio of 0.9-1.1 in sand. Binder has specific surface of 4500-5000 sq. cm and composition components are as follows, wt %: portland cement, 30.7-35.00; sand, 4.4- 9.7; wood filler, 31.8-34.0; calcium chloride, 4.2-5.7; and water, 22.5-24.0. EFFECT: arbolite mix has compression strength by 1.2-1.5 times greater than that of the prototype and consumption of portland cement is reduced by 1.4-24%. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING GAS CONCRETE MIX | 1999 |
|
RU2162069C1 |
MIXTURE FOR PRODUCTION OF MELT REFRACTORY MATERIALS | 1992 |
|
RU2081094C1 |
SLIP COMPOUND | 1996 |
|
RU2095330C1 |
CERAMIC MIXTURE FOR MANUFACTURING WALL BRICK ARTICLES | 2002 |
|
RU2230047C1 |
ELECTROLYTE FOR MANUFACTURE OF COATS OF REFRACTORY METALS | 1992 |
|
RU2061105C1 |
BLACK GLASS | 1993 |
|
RU2049746C1 |
METHOD OF PREPARING FACING CERAMIC TILES | 1995 |
|
RU2093491C1 |
RAW MIXTURE TO OBTAIN GRANULAR HEAT INSULATING MATERIAL | 2013 |
|
RU2532112C1 |
ARBOLITE BLOCK | 2021 |
|
RU2776655C1 |
METHOD OF MANUFACTURE OF HEAT-INSULATING MEMBER OF PIPE LINE | 2002 |
|
RU2215233C1 |
Authors
Dates
1999-10-20—Published
1998-01-27—Filed