FIELD: buildings, coal mines and combustible components and structures. SUBSTANCE: described is fireproof coating of wood comprising liquid glass, mineral binder and it also comprises sodium hydroxide and water, and mineral binder is sodium aluminate, ratios of components being as follows, wt %: liquid glass, 79-82; mineral binder, 0.5-0.62; sodium hydroxide, 2.4-3.3; and the water balance. EFFECT: high fireproof properties such as water resistance, strength, high adhesive power, shorter hardening and drying time of the coating. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIX FOR PREPARING FIREPROOF COATING | 1998 |
|
RU2140401C1 |
COMPOSITION FOR MAKING HEAT-INSULATING MATERIAL | 1998 |
|
RU2148046C1 |
FIRE-RESISTANT COATING COMPOSITION | 2010 |
|
RU2435810C2 |
METHOD OF OBTAINING REFRACTORY COATING | 1991 |
|
RU2016767C1 |
CRUDE MIXTURE FOR MAKING FIREPROOF COATING | 2015 |
|
RU2613515C1 |
METHOD OF LOCAL FIRE SUPPRESSION OF PEAT FIRES AND QUICK-SETTING FOAM FOR LOCALIZATION OF PEAT FIRE COMBUSTION SOURCES | 2016 |
|
RU2645542C2 |
METHOD OF PRODUCTION OF FLAME-RETARDANT COATING | 1991 |
|
RU2038977C1 |
COATING COMPOSITION | 0 |
|
SU1807037A1 |
FIREPROOF EXPANDING COMPOUND | 0 |
|
SU1293149A1 |
FIRE-RESISTANT THERMAL-PROTECTIVE COATING AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2523818C1 |
Authors
Dates
1999-11-10—Published
1998-12-24—Filed