FIELD: textile industry. SUBSTANCE: yarn contains polyester, polyacrylonitrile and viscose or high-modulus viscose filaments with linear density of 0.22-0.44 tex and length of 20-70 mm, 10-20% wt of modified linen filament with linear density of 0.7-1.5 tex and length of 20-70 mm and 5-15% wt of colored cotton combings. Share of chemical filaments in yarn is 75% wt. Method for producing yarn from mixed filaments involves forming roving by means of chemical filament processing equipment providing the number of twists of 22-26 per 1 m and spindle rotational speed of 800-1,100 min-1; forming yarn with linear density of 25-50 tex at spindle rotational speed of 7,500-10,000 min-1. According to other embodiment, method involves forming twist yarn with linear density of 50-100 tex from yarn with linear density of 25-50 tex at rotational speed of spindles on spinning-twisting machine of 6,000-7,500 min-1. Yarn of such structure may be used for manufacture of fabric for sewing of garments, as well as knitted products. EFFECT: wider range of products manufactured from such yarn, improved appearance and increased consumer qualities of yarn and products. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
YARN FOR WOVEN AND KNITTED PRODUCTS AND YARN MANUFACTURE METHOD | 1998 |
|
RU2161215C2 |
METHOD FOR PRODUCING YARN FOR WOVEN AND KNITTED ARTICLES | 1998 |
|
RU2158325C2 |
METHOD FOR PRODUCING MIXED YARN FOR WOVEN AND KNITTED ARTICLES (VERSIONS) | 1999 |
|
RU2158790C1 |
KNITTED FABRIC | 1999 |
|
RU2177516C2 |
METHOD FOR PREPARATION OF COMPOSITE YARN FOR KNITTED FABRIC | 1993 |
|
RU2061806C1 |
YARN FOR WOVEN AND KNITTED ARTICLES (VERSIONS) | 1995 |
|
RU2101398C1 |
METHOD FOR PRODUCING YARN FROM ARSELON FIBERS | 2000 |
|
RU2176293C1 |
MIXED YARN FOR LOOMWORK AND KNITTED WEAR AND METHOD FOR ITS PRODUCTION | 2001 |
|
RU2180025C1 |
METHOD FOR PRODUCING YARN FROM MIXED FILAMENTS (VERSIONS) | 1994 |
|
RU2089682C1 |
WEAR-RESISTANT FABRIC | 1993 |
|
RU2085634C1 |
Authors
Dates
2001-01-27—Published
1999-11-11—Filed