FIELD: oil and gas production. SUBSTANCE: aqueous composition containing 38.78-51.58% Portland cement, 6.39-17.80% thinning and expanding additive (hollow microspheres with 80-90% aluminosilicate component) additionally includes 10-20% aluminum hydroxychloride. EFFECT: achieved expansion effect in early period of cement stone formation owing to increased sedimentation stability of solution. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
AERATED CEMENT MORTAR COMPOSITION | 1999 |
|
RU2169828C1 |
GROUTING ADMIXTURE | 2002 |
|
RU2224876C1 |
EXPANSION COMPOSITION FOR GROUTING MORTAR | 2008 |
|
RU2387690C1 |
LIGHTENED CEMENTING SOLUTION, CEMENTING SOLUTION FOR PRODUCTIVE ZONE OF WELL AND METHOD FOR CEMENTING WELLS | 2004 |
|
RU2255204C1 |
COMPLEX REAGENT FOR GROUTING MORTARS | 2002 |
|
RU2213204C1 |
DRY LIGHT-WEIGHT PLUGGING MIXTURE | 2001 |
|
RU2209931C2 |
REAGENT FOR GROUTING MORTAR AND GROUTING MORTAR | 2007 |
|
RU2359004C2 |
COMPLEX REAGENT FOR GROUTING MORTAR AND GROUTING MORTAR | 2004 |
|
RU2259468C1 |
COMPLEX EXPANDING ADMIXTURE FOR CEMENTING SOLUTIONS | 2002 |
|
RU2230884C2 |
LIGHT POLYMER BACKFILL COMPOUND FOR OIL AND GAS WELLS | 2005 |
|
RU2288250C1 |
Authors
Dates
2001-04-10—Published
1999-08-13—Filed