FIELD: backfill solutions used during cementing of casing strings of gas, gas-condensate and oil wells, abnormal due to presence of weakly connected permafrost rocks prone to hydro-disruption.
SUBSTANCE: light polymer backfill compound for oil and gas wells includes backfill Portland cement, aluminosilicate hollow micro-spheres, polymer binding agent, hardening agent, expanding admixture. As polymer binding agent compound contains specified brand of epoxide resin and specified brand of epoxide-urethane rubber, and as hardening agent compound contains polyethylene-polyamine and oligomer amide-amine of specified brand, as expanding admixture - polyvinylchloride and dioctylphthalate plasticizer, with following ratio of components in shares of mass: resin - 31,3-42,9, dioctylphthalate - 3,6-7,5, epoxide-urethane rubber - 3,2-6,4, backfill Portland cement 13,6-24,3, aluminosilicate hollow micro-spheres - 0,6-3,8, polyvinylchloride - 13,6-22,9, polyethylene-polyamine - 1,6-2,7, oligomer amide-amine - 7,2-18,7.
EFFECT: increased strength and adhesion properties of backfill stone, decreased heat conductivity coefficient with minimal density of backfill solution equal to 1100 kg/m3 and expansion ratio equal to 0,1%.
3 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ELIMINATION OF INTERNAL GAS SHOWINGS IN WELL | 2008 |
|
RU2373377C1 |
LIGHT-WEIGHT GROUTING MORTAR | 2005 |
|
RU2303048C1 |
METHOD OF LIQUIDATION OF LEAKINESS OF WORKING STRING OF OIL AND GAS RECOVERY WELL | 2007 |
|
RU2333346C1 |
COLD-CURED EPOXY COMPOSITION | 2018 |
|
RU2749379C2 |
ABANDONMENT METHOD FOR WELL WITH GAS SHOW IN TUBING-CASING ANNULUS | 2005 |
|
RU2305754C2 |
LIGHT-WEIGHT OIL-WELL CEMENT MIX (VARIANTS) | 2003 |
|
RU2256774C2 |
COLD-CURED EPOXY BINDER | 2018 |
|
RU2749380C2 |
METHOD FOR PREVENTING OCCURRENCE OF INTER-CASING AND INTER-LAYER FLOWS IN WELL | 2023 |
|
RU2808074C1 |
LIGHT-WEIGHT GROUTING MORTAR | 2004 |
|
RU2272125C1 |
PLUGGING COMPOSITION | 0 |
|
SU1266967A1 |
Authors
Dates
2006-11-27—Published
2005-05-20—Filed