FIELD: mining.
SUBSTANCE: reagent for grouting mortar on mineral binding contains aluminium hydroxychloride, additionally contains amorphous aluminium oxide or aluminium hydroxide or their mixture at following ratio of components, wt part: aluminium hydroxychloride - 40-60, and amorphous aluminium oxide or aluminium hydroxide or their mixture - 40-60. The grouting solution contains cement, water and the said reagent at amount of from 0.5 to 3.0% from cement weight. Additionally the said grouting solution can contain in wt % from cement: filtrate agent - 0-0.8, plasticiser - 0-0.5, and de-foaming agent - 0-0.5.
EFFECT: creation of efficient reagent for grouting mortar not influencing its flow characteristics and facilitating forming of solid stone with increased resistance to deformation.
3 cl, 9 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
GROUTING MORTAR REAGENT, GROUTING MORTAR AND WELL CEMENTING METHOD | 2004 |
|
RU2268989C2 |
LIGHTENED CEMENTING SOLUTION, CEMENTING SOLUTION FOR PRODUCTIVE ZONE OF WELL AND METHOD FOR CEMENTING WELLS | 2004 |
|
RU2255204C1 |
COMPLEX REAGENT FOR GROUTING MORTAR AND GROUTING MORTAR | 2004 |
|
RU2259468C1 |
COMPLEX REAGENT FOR GROUTING MORTARS | 2002 |
|
RU2213204C1 |
EXPANSION COMPOSITION FOR GROUTING MORTAR | 2008 |
|
RU2387690C1 |
GROUTING ADMIXTURE | 2002 |
|
RU2224876C1 |
THINNED PLUGGING COMPOSITION | 1999 |
|
RU2165006C1 |
BASE COMPOSITION FOR BOS GROUTING MORTARS, GROUTING MORTAR AND METHOD OF WELL CEMENTING | 2001 |
|
RU2204693C2 |
GROUTING MORTAR | 1994 |
|
RU2082872C1 |
WELL-PLUGGING COMPOUND FOR STEAM-INJECTION WELLS | 2001 |
|
RU2220275C2 |
Authors
Dates
2009-06-20—Published
2007-07-10—Filed