FIELD: petroleum storage tanks. SUBSTANCE: inside surface of tank bottom is protected against local microbiological and hydrogen sulfide corrosion by applying thick-layer clay-based coating. Coating is composed of, wt %: bentonite clay 50.0-60.0, oil-well cement 8.0-11.0, corrosion inhibitor 2.0-5.0, water-soluble bactericide 0.005-0.1, and water -. the balance. EFFECT: simplified procedure. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROTECTION OF INNER SURFACE OF RESERVOIR BOTTOM FROM CORROSION | 1999 |
|
RU2165479C2 |
METHOD OF PROTECTION OF INNER SURFACE OF RESERVOIR BOTTOM AGAINST CORROSION | 2001 |
|
RU2221083C2 |
METHOD OF TREATING BOTTOM-HOLE FORMATION ZONE AND REGULATION OF PERMEABILITY OF WATER-OIL-SATURATED RESERVOIR | 2000 |
|
RU2166621C1 |
METHOD FOR PROTECTING OF WELL EQUIPMENT AND WELL DISCHARGE LINE | 1999 |
|
RU2170287C2 |
TECHNOLOGICAL LIQUID FOR PERFORATION AND SUPPRESSING OF WELLS | 1997 |
|
RU2115686C1 |
METHOD FOR CONTROLLING PERMEABILITY OF NOT UNIFORM OIL DEPOSIT | 2002 |
|
RU2224879C1 |
COMPOSITION FOR REMOVING ASPHALT-TAR-PARAFFIN AND BACTERIAL DEPOSITS | 2004 |
|
RU2261886C1 |
PIPELINE CORROSION PROTECTION METHOD | 1999 |
|
RU2158786C1 |
METHOD FOR WATERED NON-UNIFORM OIL RESERVOIR PERMEABILITY TREATMENT | 2005 |
|
RU2302519C2 |
METHOD FOR ISOLATING BEDS DURING FASTENING OF OPERATION COLUMN | 2005 |
|
RU2295626C2 |
Authors
Dates
2001-05-27—Published
1999-03-11—Filed