FIELD: precious metals technology. SUBSTANCE: starting material is dissolved in sulfite solution and heated. Reduction of silver is carried out in presence of alkali with paraformaldehyde reducing agent consumed in amounts of 0.27-0.35 g per 1 g silver. EFFECT: reduced residual concentration of silver in solution. 1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING SILVER FROM INDUSTRIAL PRODUCTS CONTAINING SILVER CHLORIDE | 2000 |
|
RU2185452C2 |
PROCEDURE FOR PRODUCTION OF REFINED SILVER | 2010 |
|
RU2421529C1 |
METHOD OF PROCESSING CHLORIDE SLAG CONTAINING NOBLE METALS | 1998 |
|
RU2153014C1 |
METHOD OF PROCESSING CHLORIDE SLAG CONTAINING PRECIOUS METALS | 1998 |
|
RU2150521C1 |
METHOD FOR PRODUCING REFINED SILVER FROM INTERMEDIATE PRODUCTS OF PRECIOUS METAL PRODUCTION CONTAINING SILVER IN THE FORM OF CHLORIDE | 2021 |
|
RU2779554C1 |
METHOD OF PROCESSING GOLD ALLOY | 1998 |
|
RU2151210C1 |
METHOD OF PRODUCTS REPROCESSING, CONTAINING CHALCOGENIDES OF BASE METALS, LEAD, PLATINUM METALS, GOLD AND SILVER | 2007 |
|
RU2355792C2 |
METHOD OF SILVER RECEIVING | 2008 |
|
RU2378398C2 |
SILVER AFFINAGE METHOD | 1995 |
|
RU2100457C1 |
METHOD OF PROCESSING PRODUCTS CONTAINING CHALCOHENIDES OF NON-NOBLE METALS, LEAD, METALS OF PLATINUM GROUP, GOLD AND SILVER | 2005 |
|
RU2291212C1 |
Authors
Dates
2001-07-10—Published
1999-07-15—Filed