FIELD: nonferrous metallurgy. SUBSTANCE: sodium hydroxide is admixed to molten lead at 340-370 C in proportion 0.2-0.3% of the weight of lead. Thereafter, 0.03-0.06% sodium sulfide and simultaneously 0.05-0.1% elementary sulfur are introduced into funnel formed on the surface of stirred melt to give double copper-sodium sulfide having lower solubility in liquid lead than sodium sulfide. The latter emerges on the surface of metal and is removed after each portion of sulfur-containing reagents admixed to melt. Sulfur-containing reagents are added 1 to 4 times depending on content of copper in initial material. Residual content of copper in lead is equal to or below 0.001%. EFFECT: provided fine decopperization of lead within sufficiently wide temperature range in melt containing no tin and silver. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF LEAD REFINING | 0 |
|
SU901317A1 |
METHOD OF PROCESSING FINE-GRAIN LEAD AND LEAD-ZINC COPPER-CONTAINING SULFIDE CONCENTRATES | 0 |
|
SU1544829A1 |
METHOD FOR REFINING LEAD FROM COPPER AND CENTRIFUGAL APPARATUS FOR ITS IMPLEMENTATION | 2016 |
|
RU2630070C2 |
METHOD FOR EXTRACTING LEAD FROM SECONDARY RAW MATERIAL | 2001 |
|
RU2208057C1 |
METHOD OF ASSAY DETERMINATION OF CONTENT OF GOLD IN ORES AND IN PRODUCTS OF THEIR PROCESSING | 2005 |
|
RU2288288C1 |
METHOD FOR REMOVING COPPER FROM BLACK LEAD | 0 |
|
SU1138423A1 |
METHOD OF PROCESSING UNDERWATER IRON-MANGANESE ORES | 2001 |
|
RU2184163C1 |
CUPEL LITHARGE REPROCESSING METHOD | 1992 |
|
RU2041275C1 |
COMBINED METHOD OF PROCESSING TAILINGS OF CONCENTRATION OF POLYMETALLIC ORES | 1998 |
|
RU2197547C2 |
METHOD OF EXTRACTION OF SILVER FROM LEAD-TIN ALLOYS | 1999 |
|
RU2154688C1 |
Authors
Dates
2001-12-20—Published
2001-02-14—Filed