FIELD: production of bars from pseudo--β- titanium alloys for manufacture of bolts. SUBSTANCE: rolling of bars is performed in β- area at two stages; final rolling performed in (α+β)--area is accompanied by air cooling after each deformation. Rolling parameters are as follows: first stage - heating to Trp + (40-150)C, deformation degree, 97 to 97.6 %; second stage - heating to Trp +20C, deformation degree, 37 to 38 %; final rolling - heating to Trp - (20-50)C, deformation degree, 54 to 55 %. EFFECT: possibility of obtaining microstructures of 1-2 type acc. to scale; possibility of obtaining strength of no less than 85 kgf/sq. mm and conducting cold upsetting at degree of 75 %. 6 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING BARS AND STRIPS FROM COMMERCIAL TITANIUM | 2000 |
|
RU2175994C2 |
METHOD FOR MAKING ROLLED BARS OF TITANIUM ALLOYS | 1999 |
|
RU2175581C2 |
METHOD OF MAKING HOLLOW TUBULAR BLANK FOR PRODUCING SEAMLESS TUBES FROM PSEUDO-ALPHA AND (ALPHA+BETA)-TITANIUM ALLOYS | 1998 |
|
RU2127160C1 |
METHOD FOR MAKING INTERMEDIATE BLANKS OF α AND α TITANIUM ALLOYS | 2002 |
|
RU2217260C1 |
METHOD FOR MAKING THIN SHEETS OF HIGH-STRENGTH TITANIUM ALLOYS | 2003 |
|
RU2250806C1 |
METHOD FOR MAKING INTERMEDIATE BLANK OF (α+β) TITANIUM ALLOYS | 2004 |
|
RU2266171C1 |
METHOD FOR MAKING ROLLED BARS | 1999 |
|
RU2165808C1 |
METHOD FOR MAKING ONE-PIECE ROLLED WHEELS OF TITANIUM ALLOYS | 2003 |
|
RU2236322C1 |
METHOD OF HOT ROLLING OF TITANIUM-ALLOY RODS | 1997 |
|
RU2108876C1 |
METHOD FOR MANUFACTURING RODS OF TITANIUM BASED ALLOYS | 2015 |
|
RU2644714C2 |
Authors
Dates
2002-01-10—Published
2000-05-06—Filed