FIELD: investment casting of blades of gas-turbine engines and other parts of complicated configuration. SUBSTANCE: composition contains solid hydrocarbon and/or wax in amount of 0.1-80 wt.% and/or polymer with melting temperature up to 300 C in amount of 0.05-30 wt.%, and also thermopolymer resin in amount of up to 100 wt.%. Introduction of thermopolymer resin increases strength of composition and reduces linear shrinkage. EFFECT: increased technological effectiveness and usefulness of composition for wide nomenclature of patterns with higher geometric accuracy. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR MANUFACTURING MELTED PATTERNS | 2000 |
|
RU2177387C1 |
COMPOSITION FOR CASTING INVESTMENT PATTERNS | 2010 |
|
RU2447968C1 |
COMPOSITION FOR MANUFACTURING INVESTMENT PATTERNS | 2000 |
|
RU2162386C1 |
COMPOSITION FOR CASTING INVESTMENT PATTERNS | 2015 |
|
RU2600468C2 |
COMPOSITION FOR CASTING INVESTMENT PATTERNS | 2010 |
|
RU2447969C1 |
COMPOSITION FOR MAKING INVESTMENT PATTERNS | 0 |
|
SU1342583A1 |
COMPOSITION FOR MAKING SMELTING ARTICLES | 0 |
|
SU1117117A1 |
CERAMIC CORE STRENGTHENING METHOD | 2002 |
|
RU2232664C1 |
METHOD OF MAKING CERAMIC MOULDS BY FUSIBLE PATTERNS | 2012 |
|
RU2499651C1 |
CHARGE FOR REFRACTORY ARTICLE MAKING | 2001 |
|
RU2191167C1 |
Authors
Dates
2002-05-10—Published
2000-05-31—Filed