FIELD: leather industry. SUBSTANCE: method involves chrome tanning. Treatment of semifinished product is carried out with copolymer of acrylamide, methacrylic acid and acrylic acid nitrile taken in the ratio = (40-60): (20- 30): (20-30), respectively, taken in amount 1.0-3.0% of semifinished product mass followed by additional tanning with chrome tanning agent and neutralization. Invention can be used for production of leather for different aims. EFFECT: enhanced strength properties of leather. 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING NATURAL LEATHERS | 2001 |
|
RU2184785C1 |
SKIN TREATMENT METHOD | 2002 |
|
RU2213786C1 |
SKIN TREATMENT METHOD | 2001 |
|
RU2186116C1 |
METHOD OF LEATHER MAKING | 1997 |
|
RU2112042C1 |
METHOD OF LEATHER TREATMENT | 2002 |
|
RU2193601C1 |
LEATHER MANUFACTURE PROCESS | 1998 |
|
RU2129164C1 |
METHOD OF LEATHER MAKING | 1997 |
|
RU2113493C1 |
METHOD OF LEATHER MAKING | 1996 |
|
RU2096474C1 |
METHOD OF TREATMENT OF POULTRY HIDES | 2002 |
|
RU2193602C1 |
METHOD OF MANUFACTURING NATURAL PILE LEATHER | 2003 |
|
RU2225451C1 |
Authors
Dates
2002-05-20—Published
2001-10-16—Filed