FIELD: polymer materials. SUBSTANCE: siloxane rubber-based composition with reinforcement filler (Aerosil) containing curing initiator (peroxide) and inert filler (modified fine aluminum hydroxide) is prepared by consecutively adding composition components at 20-40 C on rollers which are spaced by 1.0-6.0 mm from each other. EFFECT: improved electric and physico-mechanical properties of polymer composition used for manufacturing high-voltage external- construction apparatuses. 10 cl, 2 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
INSULATOR, SURGE LIMITER, AND METHOD FOR MANUFACTURING POLYMERIC SHELL | 1999 |
|
RU2203514C2 |
HEAT-RESISTANT ELECTRICALLY INSULATING COMPOSITION BASED ON POLYDIMETHYL VINYL SILOXANE RUBBER | 2010 |
|
RU2445329C1 |
FIRE-RESISTANT RUBBER MIXTURE | 2012 |
|
RU2540597C2 |
FIRE-RESISTANT RUBBER MIXTURE | 2011 |
|
RU2472821C1 |
CERAMICS-FORMING RUBBER MIXTURE (VERSIONS) | 2012 |
|
RU2519379C2 |
COMPOSITE MATERIAL FOR PRODUCING COMPOSITE MATERIALS | 2013 |
|
RU2516500C1 |
OIL-, GASOLINE-, FIRE-, AND FROST-RESISTANT RUBBER-INSULATED ELECTRIC DRIVE | 2004 |
|
RU2249869C1 |
POLYMER TWO-COMPONENT COMPOSITION | 2018 |
|
RU2700684C1 |
VIBRO-DAMPING ELASTOMERIC MATERIAL OF HIGH DENSITY | 2016 |
|
RU2631789C1 |
COMPOSITE FOR PRODUCTION OF GENERAL MECHANICAL RUBBER GOODS | 2004 |
|
RU2285703C2 |
Authors
Dates
2002-08-10—Published
1999-08-24—Filed