FIELD: building materials. SUBSTANCE: method involves rubble impregnation at room temperatures with sleeper-impregnating composite (coal oil, shale oil or their mixtures) under excessive pressure 0-6.0 MPa for 120-300 s and the following its stirring with 3.0% of melted rubble of rubble mass up to uniform material covering. The application of such method ensures to reduce rubble crushability (rubble loss at standard thickening) as compared with control (known) methods in average by 2.46-3.72-fold and water absorption after experiments for standard thickening by 2.23-3.96-fold. Invention can be used for bases and covers making in automobile roads. EFFECT: improved method of preparing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING BLACK CRUSHED STONE | 2001 |
|
RU2204538C2 |
METHOD OF PREPARING BLACK CHIPPINGS | 2011 |
|
RU2461522C1 |
PRODUCTION OF BLACK CRUSHED ROCK | 2014 |
|
RU2552286C1 |
METHOD OF PREPARING BLACK CRUSHED ROCK | 0 |
|
SU1520043A1 |
METHOD OF PREPARING CONSTRUCTION LIMESTONE CHIPS | 2009 |
|
RU2408550C1 |
METHOD OF PRODUCING STRUCTURAL MATERIALS FROM STONE CRUSHING CARBONATE WASTES | 2011 |
|
RU2494056C2 |
METHOD FOR PREPARING LIMESTONE LOW-STRENGTH CRUSHED STONE | 2022 |
|
RU2792129C1 |
METHOD OF PREPARING BINDER FOR ROAD BUILDING | 1997 |
|
RU2128632C1 |
ASPHALTIC CONCRETE MIX | 2001 |
|
RU2204539C2 |
METHOD OF PREPARING LIMESTONE CONSTRUCTION RUBBLE | 2016 |
|