FIELD: construction.
SUBSTANCE: method of preparing limestone construction rubble includes preheating limestone construction rubble to a temperature of 50-60°C, impregnating the heated rubble in an aqueous solution of lignosulfonates at the ratio of lignosulfonates: water, respectively, 1:(8-12) at intensive stirring for 20-30 mines, followed by drying the rubble at a temperature of 100-110°C to a constant weight.
EFFECT: increasing the strength characteristics of limestone construction rubble while reducing the impregnation time and reducing energy costs.
1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING CONSTRUCTION LIMESTONE CHIPS | 2009 |
|
RU2408550C1 |
METHOD OF PREPARING LIMESTONE CONSTRUCTION RUBBLE | 2017 |
|
RU2645030C1 |
METHOD FOR PREPARING LIMESTONE LOW-STRENGTH CRUSHED STONE | 2022 |
|
RU2792129C1 |
METHOD OF PRODUCING STRUCTURAL MATERIALS FROM STONE CRUSHING CARBONATE WASTES | 2011 |
|
RU2494056C2 |
METHOD OF PREPARING A MODIFIED BUILDING LIMESTONE CRUDE | 2017 |
|
RU2668902C1 |
METHOD OF PREPARING BLACK CRUSHED STONE | 2001 |
|
RU2204538C2 |
METHOD FOR PRODUCING SULPHUR-IMPREGNATED CHIPPINGS FOR CONSTRUCTION OF ROAD BASES AND PAVINGS AND UNIT FOR PRODUCTION OF SULPHUR-IMPREGNATED CHIPPINGS | 2023 |
|
RU2805450C1 |
METHOD OF PREPARING BLACK CHIPPINGS | 2011 |
|
RU2461522C1 |
METHOD OF BLACK RUBBLE PREPARING | 2001 |
|
RU2200717C2 |
PRODUCTION OF BLACK CRUSHED ROCK | 2014 |
|
RU2552286C1 |
Authors
Dates
2018-01-25—Published
2016-11-15—Filed