FIELD: carbon materials. SUBSTANCE: active and moderately active brands of kiln carbon black are produced from liquid hydrocarbon stock subjected to thermal decomposition in reactor, combustion chamber of which receives fuel and air. According to invention, before feeding into reactor, hydrocarbon stock is completed by water, which is added at weight ratio to hydrocarbon stock (88-98.5): (1.5-12), after which resulting mixture is emulsified in hydrodynamic activator during 2 to 180 sec or in flow mixer during 90 to 270 sec, thus obtained emulsion is heated to 120-300 C and introduced in sprayed state into reactor. Advantageously, thermal decomposition of hydrocarbon stock is conducted at 1200-1600 C. EFFECT: increased yield of carbon black (by 2-8%). 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FEEDSTOCK FOR PRODUCTION INDUSTRIAL CARBON | 1999 |
|
RU2168526C2 |
RAW MATERIAL FOR PRODUCTION OF HALF-ACTIVE AND LOW-ACTIVE CARBON BLACK | 2001 |
|
RU2206586C2 |
METHOD OF PRODUCING SEMI-ACTIVE TECHNICAL CARBON | 2015 |
|
RU2614964C1 |
RAW COMPOSITION FOR CARBON BLACK PRODUCTION | 2001 |
|
RU2198192C2 |
METHOD OF PRODUCING LOW-DISPERSED TECHNICAL CARBON AND REACTOR FOR REALISING SAID METHOD | 2010 |
|
RU2446195C1 |
METHOD OF PRODUCING SEMI-ACTIVE TECHNICAL CARBON AND REACTOR FOR REALISING SAID METHOD | 2008 |
|
RU2394054C2 |
METHOD OF PRODUCTION OF TECHNICAL CARBON | 2002 |
|
RU2200746C1 |
METHOD OF PRODUCTION OF OIL-HEAT- TRANSFER AGENT | 2002 |
|
RU2216570C1 |
HEAVY HYDROCARBON FEEDSTOCK PROCESSING METHOD | 2002 |
|
RU2215020C1 |
METHOD FOR MAKING CARBON BLACK, HYDROCARBON PROPELLANTS AND CHEMICAL STOCK OF RUBBER-CONTAINING INDUSTRIAL AND HOUSEHOLD WASTE | 2006 |
|
RU2352600C2 |
Authors
Dates
2003-05-27—Published
2001-05-25—Filed