FIELD: heat-protection materials. SUBSTANCE: two-layer coating is formed on fabric substrate by applying siliconorganic rubber-based composition followed by drying of each layer of coating. Utilized fabric is made from extra-strong fibers, breaking strength of fabric being at least 1000 N for warp, and at least 800 N for shute, and surface density of fabric being at least 100 g/sq.m, preferably 100-170 g/sq.m. Composition is supplemented by silica powder and hardener. Coating layers are dried at 170-220 C. Internal layer, adjoining substrate and representing 40-75% of the total coating weight, has density 30-70 g/sq.m and outside layer, adjoining internal one and representing 25-60% of the total coating weight, has density 25-45 g/sq.m. For manufacture of material, silicon-organic rubbers are used characterized by working temperature range from -50 C to +250 C and viscosity at least 16000 vPa. s. EFFECT: increased strength, fire and frost resistances, and waterproofness. 5 cl, 1 tbl, 4 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF MANUFACTURING HEAT-RESISTANT MATERIAL | 2002 | 
 | RU2206652C1 | 
| HEAT-RESISTANT MATERIAL MANUFACTURE METHOD | 2002 | 
 | RU2210647C1 | 
| POLYMERIC HEAT-REFLECTING COATING COMPOSITION | 2011 | 
 | RU2467042C1 | 
| THERMAL-RESISTANT POLYMER HEAT-REFLECTING COMPOSITION WITH LOW EMISSIVITY | 2016 | 
 | RU2633900C1 | 
| TWO-LAYER PROTECTIVE FABRIC | 2016 | 
 | RU2647807C1 | 
| BACTERICIDAL ORGANOSILICON SEALANT | 2011 | 
 | RU2486222C2 | 
| MULTI-LAYER MATERIAL FOR FLYING VEHICLE ENVELOPES AND METHOD OF MANUFACTURE OF SUCH MATERIAL | 2003 | 
 | RU2228850C1 | 
| HEAT-REFLECTING FIREPROOF LAMINAR RUBBERISED FABRIC PROTECTIVE MATERIAL | 2012 | 
 | RU2496647C1 | 
| FIREPROOF HEAT-PROTECTIVE MATERIAL | 2014 | 
 | RU2559499C1 | 
| POLYMERIC POLYURETHANE COMPOSITION AND MULTILAYER MATERIAL BASED THEREON | 2012 | 
 | RU2494131C1 | 
Authors
Dates
2003-08-20—Published
2002-04-29—Filed