FIELD: explosives. SUBSTANCE: pyrotechnic composition that can be used in heating elements as heat source contains tungsten trioxide, titanium powder, and molybdenum disulfide. Composition is characterized by friction sensitivity 6-14, specific heat emission 1500-2000 J/g, and gas emission 3.5-9 cu.cm/g. EFFECT: improved performance characteristics. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RETARDING PYROTECHNIC COMPOUND (VERSIONS) | 2005 |
|
RU2291141C1 |
RETARDING COMPOSITION (VERSIONS) | 2006 |
|
RU2332393C2 |
PYROTECHNICAL COMPOSITION | 2011 |
|
RU2483050C2 |
PYROTECHNIC COMPOSITION | 2005 |
|
RU2297404C1 |
PYROTECHNIC RETARDING COMPOSITION | 2002 |
|
RU2225385C2 |
GAS-FORMING PYROTECHNICAL COMPOSITION | 1998 |
|
RU2151759C1 |
PYROTECHNIC COMPOSITION | 2013 |
|
RU2531293C1 |
GAS-GENERATING PYROTECHNIC COMPOSITION | 1993 |
|
RU2068831C1 |
COMPOSITION FOR MANUFACTURING ELASTIC PYROTECHNIC MATERIAL | 2005 |
|
RU2306306C2 |
EXOTHERMIC COMPOSITION FOR HEATING ELEMENT | 2019 |
|
RU2717227C1 |
Authors
Dates
2004-01-27—Published
2001-12-24—Filed