FIELD: inorganic compounds technology. SUBSTANCE: aluminosilicate raw material is treated with sulfuric or hydrochloric acid, resulting solution is supplemented by 15-30% of concentrated sulfuric or hydrochloric acid and heated to 35-80 C for 10-120 min until coagulant containing 10 to 95% of polymer forms of silica is obtained. EFFECT: improved coagulating and flocculating properties. 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ALUMINOSILICATE COAGULANT | 1995 |
|
RU2088527C1 |
METHOD OF OBTAINING COAGULANT-FLOCCULANT | 2010 |
|
RU2471720C2 |
METHOD OF PRODUCING ALUMOSILICIC COAGULANT-FLOCCULANT | 2009 |
|
RU2421400C1 |
METHOD FOR OBTAINING CALCIUM ALUMINOSILICATE INORGANIC COAGULANT | 2018 |
|
RU2683082C1 |
METHOD OF PREPARING COAGULATION-FLOCCULATION REAGENT AND WATER TREATMENT PROCESS | 1997 |
|
RU2131849C1 |
METHOD FOR OBTAINING AN ALUMINUM-SILICON COAGULANT-FLOCCULANT | 2021 |
|
RU2763356C1 |
METHOD FOR PRODUCING ALUMINOSILICATE HYBRID REAGENT FOR TREATING NATURAL AND INDUSTRIAL WASTEWATER AND METHOD OF TREATING NATURAL AND INDUSTRIAL WASTEWATER WITH THIS REAGENT | 2017 |
|
RU2661584C1 |
METHOD FOR PRODUCING COAGULANT BASED ON ALUMINIUM POLYOXYSULFATE, COAGULANT PRODUCED BY SAID METHOD | 2015 |
|
RU2617155C1 |
METHOD FOR PRODUCTION OF COAGULANT | 1992 |
|
RU2039711C1 |
PAPER AND CARDBOARD MANUFACTURE PROCESS | 2000 |
|
RU2247184C2 |
Authors
Dates
2004-03-20—Published
2002-11-26—Filed